profile banner

Ivoclar | Emax Press Manual

This article serves as a comprehensive walkthrough of the official EMAX Press manual, covering everything from sprue design and investment to pressing and divesting.

The manual dedicates a full chapter to .

| Step | Procedure | Key Parameter (from manual) | |------|-----------|------------------------------| | 1 | Wax/Lithium disilicate burnout ring | 850°C (prolonged burnout) | | 2 | Plunger & ring preheating | 1–2 cycles at 850°C | | 3 | Pressing temperature | 915°C – 1050°C (depends on ingot size) | | 4 | Pressing time | 12–15 minutes | | 5 | Investment material | PressVEST Speed / Power (phosphate-bonded) | | 6 | Cooling after press | Slow bench cool to <500°C before divesting |

If you need data on long-term success or material properties, these reports are key: